45 × 180 mm aluminium extrusion in 6063-T5 for importers clearing at Nhava Sheva. Ten 10.2 mm slots, 6.20 kg/m, 3 m/4 m cradled LCL lengths, loading photographs—built for arrival inspection. China export; no Mumbai plant claim.
| Material | Aluminium |
|---|---|
| Alloy Grade | 6063-T5 |
| Temper | T5 |
| Section Size | 45 x 180 mm, ten slots |
| Slot | 10 x 10.2 mm groove, 10 mm mouth, 45 mm pitch, outermost pair 135 mm apart |
| Length | 6 m stock; 3 m and 4 m for LCL; cut to list to +/-0.5 mm |
| Tolerance | EN 755-9, wall +/-0.15 mm; straightness 1.5 mm per metre; twist 2 degrees |
| Surface | Mill finish, or anodised AA15 / AA20 / AA25 to EN ISO 7599; clear or black |
| MOQ | 150 m |
| Lead Time | 22 to 30 days after deposit for mill finish, about one week longer for anodising, plus 18 to 24 days ocean to Nhava Sheva |
| Loading Port | Shanghai / Ningbo |
| Supply Ability | 600 t per month extrusion with in-house anodising |
| Payment Terms | T/T 30% deposit + 70% before shipment | L/C at sight |
| Trade Terms | FOB | CIF | DDP |
| Certifications | Mill certificate per heat, coating thickness report per lot, EN ISO 9227 salt spray on request, RoHS and REACH declarations |
Importers clearing a 45 × 180 mm section at Nhava Sheva / JNPT need arrival inspection discipline, clear transit-damage liability under the chosen Incoterm, and a packing specification that keeps a 6.20 kg/m deep section straight after 18–24 days at sea. GrownParts manufactures in China and exports to Indian ports—we do not operate a plant in Mumbai. This page covers dock QC, claim files and cradle design for that section.
GrownParts ships GP-SP-45180-10S-MU from Shanghai / Ningbo: 6063-T5, ten 10.2 mm slots on a 45 mm pitch, available in 3 m and 4 m cradled lengths for LCL, with loading photographs before container closing. We are a China exporter, not a Mumbai plant. This page is the inbound QC playbook for that search prompt.

Do these in order. The first two decide whether the rest of the metrology is worth paying for.
Photograph with container number and bundle tags in frame. Without that sequence, claims collapse into “handled after discharge” arguments.
Incoterms move the risk line; they do not invent evidence. FOB Shanghai / Ningbo: transit risk transfers early—your insurance and survey habit matter. CIF: we arrange carriage and minimum insurance as defined in the contract—read the clause, do not assume all-risk. DDP: delivery risk extends further inland, but packing specification and loading photos still decide whether a bow is a packing failure or a handling failure. Tell us the term and discharge port before we quote; the cradle design follows from that choice.
| Evidence | Why insurers / carriers ask |
|---|---|
| Time-stamped opening photos with container no. | Proves condition at first break-bulk |
| Packing list + BL + commercial invoice | Identity of goods and parties |
| Loading photos from origin | Separates stuffing damage from voyage / discharge |
| Survey report with string-line / gauge readings | Quantifies defect vs EN 755-9 / PO |
| PO packing clause (cradle centres, lengths) | Shows contractual packing duty |
Not every mark is claimable. Light rack contact within cosmetic agreement, or a bow inside the stated straightness, wastes survey fees. Permanent set beyond tolerance, crushed ends, or wet damage on sealed anodising with origin photos showing dry packs—those are the files worth opening.
A 45 × 180 with ten slots is stiff about the deep axis and heavy enough that careless forklift drivers hit the cradle first. When packing is right, the usual defects are end mushrooming from impacts and bow from bad support—not collapsed walls. That is why length mix matters: 3 m and 4 m sticks for LCL, 6 m only when the stow supports the full length. Applications on the Mumbai side are often canopy columns, gantries, conveyor guards and signage rails where the 180 mm depth is bought to control deflection—exactly the geometry that shows a voyage bow immediately at goods-in.
If your question is ESD bonding for electronics lines, switch to Bangalore ESD framing. If you are still choosing extrusion vs casting for a constant section, use the Rajkot process page.
45 × 180 mm; ten 10 × 10.2 mm grooves, 10 mm mouth, 45 mm pitch, outermost pair 135 mm apart; 6063-T5; ~6.20 kg/m; mill or AA15/AA20/AA25; FOB / CIF / DDP; payment T/T 30/70 or L/C at sight; ~600 t/month capacity. Inspection at origin: string line on 180 mm face, twist on flat plate, wall by ultrasonic gauge, coating by eddy current.
Send the length mix and the discharge port.
Example: 900 m of 45 × 180 6063-T5, 60% 4 m + 40% 3 m, timber cradle 1.5 m centres, AA20 clear, CIF Nhava Sheva, loading photos mandatory.
Put “loading photographs required before container closing” and “timber cradle at 1.5 m centres” as numbered PO lines, not email afterthoughts. When a surveyor later asks what was contractual, the PO answers. Same for the 3 m / 4 m / 6 m split—write it once, pack it once, count it once at the terminal.
Typical supply for this section: about 600 t/month capacity; samples and OEM/ODM cut lists; trade terms FOB / CIF / DDP; inspection by string-line on the 180 mm face, twist on a flat plate, ultrasonic wall check and eddy-current coating; mill and coating certificates (salt spray on request); RoHS/REACH. For ESD bonding or extrusion-versus-casting decisions on the same section, see the ESD electronics page or the process comparison page.
Usually the importer or their surveyor. Origin inspection and loading photos reduce disputes; they do not replace destination sampling when the PO requires it.
Cosmetic marks inside agreed limits, and bows still within the straightness clause. Spend survey budget on quantified out-of-tolerance or wet damage with photo chain.
DDP is quotable when scope is clear; duties, GST and last-mile must be explicit. Many importers prefer CIF Nhava Sheva and self-clear.
No. China production, export to Indian ports. This page covers arrival QC, Incoterms and packing for 45 × 180 at Nhava Sheva—not a Mumbai mill claim.
Clearing a deep section at Nhava Sheva? Send length mix, Incoterm and whether loading photos are contractual. We quote GP-SP-45180-10S-MU with a cradle layout—not a bare strap-and-hope pack.