Metric Industrial Aluminium Profiles: 15 to 60 Series
A series number is a nominal size, not a specification. Three things decide whether a consignment passes incoming inspection: the section data for the exact die, the straightness class you named on the drawing, and whether the cut, tapped and labelled pieces arrive in the order your assembly line needs them. This article puts the catalogue numbers for all seven metric series next to the tolerances, the inertia figures and the fabrication limits we actually work to.

Short answer
Yes, heavy 40 × 80 and 60 × 60 metric T-slot sections can be supplied from a Chinese factory, and yes, pre-cut, end-tapped and kitted lengths can be shipped directly — but the three questions are usually answered against three different documents. The section is quoted against a die drawing. Straightness is quoted against an execution class, normally EN 755-9, which permits 1.5 mm per metre of bow and 2 degrees of twist; that is an extrusion tolerance, not a linear-rail mounting tolerance. Cutting and tapping are quoted against a fabrication drawing with its own tolerances: cut length ±0.5 mm, hole position ±0.2 mm, end square within 0.3 mm. And BOM kitting is quoted against a packing list that has to say what the label carries. In our catalogue, 40 × 80 runs from 2.10 to 3.60 kg/m depending on wall, 60 × 60 from 2.75 to 6.40 kg/m, and the standard temper is 6063-T5, with 6061-T6 on designated sections. Where a rail needs a flatness better than an extruded face can hold, the honest route is a CNC-milled datum face, not a tighter word on the purchase order.

The series number does not tell you the slot
The first mistake in a metric T-slot enquiry is writing “40 series” and assuming the hardware follows. It does not. The number describes a nominal face dimension; the slot mouth, groove depth, pitch and nut thread are properties of the die. Two sections both sold as 40 series can take different nuts, and two sections sold under different series numbers can share a nut.
Our own catalogue shows the spread. A 40 series 40 × 40 section is listed with an 8 mm mouth, 30 mm pitch and M6 slot reference, while a 40 series joining plate is listed for an 8 mm slot with M8 T-nuts. In the 45 series you find both an 8 × 8 mm groove taking M10 nuts at 33 mm pitch and a 10 mm slot taking M8 or M10. In the 50 and 60 series a single T-nut is listed for both, against a 10 mm slot and a 14 mm groove cavity. A 20 series section uses a 6.2 mm mouth and a 6 mm groove at 20 mm pitch; a 15 series section uses a 6.2 mm mouth and a 6 mm groove at 15 mm pitch. The last two differ by pitch, not by slot mouth.
So the four numbers to put on an RFQ are the slot mouth, the groove depth or cavity, the pitch between slots, and the nut thread. Add the nominal section and the wall variant. Without those, a supplier can only quote a family, and the family is not what your assembly jig bolts onto. The same caution applies to cross-brand substitution: interchangeability is a hardware question, not a dimension question, and it is covered separately in T-Slot Cross-Brand Compatibility.
| Series | Catalogue sections | Slot / groove | Pitch | Slot nut | Mass kg/m | Ix=Iy cm⁴ |
|---|---|---|---|---|---|---|
| 15 | 15 × 15; 30 × 15 three-slot | 6.2 mm mouth, 6 mm groove | 15 mm | M4 / M5 | 0.48–0.55 | Ask for the die |
| 20 | 20 × 20; 20 × 40; 20 × 80; 40 × 40 eight-slot | 6.2 mm mouth, 6 mm groove | 20 mm | M5 / M6 | 0.49–1.05 | 0.72–0.74 (20 × 20) |
| 30 | 30 × 30 light; 30 × 120 three-slot | 6 mm mouth, 4.5 × 4.5 mm groove | 30 mm | M5 / M6 | 0.95–3.10 | Ask for the die |
| 40 | 40 × 40; 40 × 60; 40 × 80 | 8 mm mouth | 30 mm | M6 / M8 | 1.30–3.60 | 8–14 (40 × 40) |
| 45 | 45 × 45 light and heavy; 45 × 90 heavy | 8 × 8 mm groove; 10 mm slot variants | 33 mm | M8 / M10 | 1.90–4.10 | ≈68 (45 × 90 heavy) |
| 50 | 50 × 50; 50 × 100 heavy; 100 × 100 eight-slot | 6.8 × 6.8 mm groove; 10 mm slot variants | 35 mm | M8 / M10 | 3.10–9.20 | Ask for the die |
| 60 | 60 × 60 standard and heavy; 60 × 60 L-section | 10.2 mm mouth, 14 × 14 mm groove | On the die drawing | M8 / M10 / M16 fixing | 2.75–6.40 | Ask for the die |
Every value above comes from a section in our own ACF catalogue, not from an industry average. We have published inertia figures for three of the seven series. We have deliberately left the other four blank rather than print a plausible number: internal webs differ enough between dies in the same series to move deflection by a full serviceability class, and a number copied from a different catalogue is worse than no number. Ask for Ix, Iy and Z on the quotation drawing for the exact die, and ask whether it was calculated from the nominal section or measured from a DXF. Our Moment of Inertia and Section Modulus of T-Slot Profiles sets out the calculation and the common errors.
Why the blanks are the useful part of that table
A supplier who fills all seven inertia cells from memory is telling you more about their sales process than their extrusion process. The section modulus and the second moment depend on where the metal sits, and a light and heavy version of the same 40 × 40 can differ by more than a kilogram per metre. If a quotation cannot produce the die drawing and the section data behind the load figure, the load figure is not a specification you can inspect against.
Load capacity: the number that scales, and the number that does not
Two section properties do the work. The second moment of area, I, governs deflection. The section modulus, Z, governs bending stress. For a simply supported member with a central point load, the screening equation is δ = F·L³/(48·E·I), with E ≈ 69 GPa for 6063-T5. Yield is rarely the first limit on a light frame; joint slip and a serviceability deflection limit trip first.
Worked to L/300 with 6063-T5, the allowable central point load in kilograms is roughly 1.14 × 10⁷ × I in cm⁴ divided by the span in millimetres squared. Take a 2,400 mm opening. A standard 40 × 40 with I ≈ 9.5 cm⁴ gives about 19 kg and fails a 250 kg gantry load. A 50 × 100 section used on edge gives about 297 kg and passes. A 45 × 90 heavy rail with I ≈ 68 cm⁴ gives about 135 kg on the same span — roughly seven times the 40 × 40 for about twice the mass per metre. That ratio is why heavy sections exist: I scales with the cube of the depth, mass only with area.
The alternative is to change the span, not the section. Three extra 40 × 40 uprights at 600 mm centres bring the same 2,400 mm run to about 301 kg allowable and add 4.6 kg of upright, against 10.8 kg more for the 50 × 100 route. Halving a span is worth four times the load in the fourth-power sense, and a diagonal in the same profile is over 300 times stiffer in axial loading than the same bar is in bending. Our T-Slot Profile Size and Geometry works through the four layouts; the load-tier map places them in a purchasing sequence.
| Section / layout | I, cm⁴ | Allowable central load, 2,400 mm, L/300 | Mass on the run | What it costs you |
|---|---|---|---|---|
| 40 × 40 standard, single span | ≈9.5 | ≈19 kg — fails 250 kg | 4.1 kg | Deflection, not strength |
| 45 × 90 heavy, single span | ≈68 | ≈135 kg | ≈9.8 kg | Depth in the machine envelope |
| 50 × 100 on edge, single span | not published here | ≈297 kg — passes | 14.9 kg | 100 mm of depth, 50 series M10 hardware |
| 40 × 40, four 600 mm spans | ≈9.5 | ≈301 kg — passes | 8.7 kg total | Three uprights and the assembly time |
For a linear rail bed, L/300 is the wrong limit before the calculation starts. Rail beds are normally screened to L/500 or to an absolute figure from the rail maker, and the load is distributed rather than a single central point. A 3 m rail through a 40 °C temperature rise also grows about 2.8 mm if it is free to move, using 23.4 µm/m·°C for 6063. State the installation temperature and the operating temperature on the drawing; a frame assembled at 10 °C and run at 50 °C near an oven needs the full swing in both directions. Bolted joints add their own compliance: keep dry torque near 5–8 Nm for M6 and 13–20 Nm for M8 and recheck after vibration, because the usual fatigue mode is fretting and preload loss at the T-nut rather than failure of the parent bar.
Straightness: what stretching fixes, and what it cannot
An extrusion leaves the press hot and curved. Quenching sets in a bow, and the standard corrective step is stretcher straightening: the section is gripped at both ends and pulled past yield by a controlled amount to even out the longitudinal stress before it is cut to stock length and aged. Straightening is a mechanical operation on the whole length. It does not machine a face, and it does not create a plane.
What you can hold is set by the execution class. We quote EN 755-9 as standard and EN 12020-2 when the drawing is marked precision. EN 755-9 permits 1.5 mm of bow per metre, 2 degrees of twist over the length and ±0.15 mm on light walls. On a 3 m rail, a class that allows 1.5 mm per metre already permits 4.5 mm of deviation. No linear guide maker wants that under a carriage, and no amount of shimming at the bolts will make a carriage travel smoothly over it. This is the gap that the phrase “tight straightness” hides in an enquiry: the buyer means a mounting surface, the supplier hears an extrusion tolerance, and both sign the same purchase order.
Uneven walls make the starting condition worse. A 1.2 mm face opposite a 3.0 mm face pulls metal to the thick side during extrusion and costs straightness before the stretcher is reached. A uniform 1.6 mm wall runs faster and straighter. It also changes which press the section needs: our envelope is seven lines from 800 to 1,500 t with a 320 mm circumscribing circle ceiling, and the minimum wall is 0.8 mm on 6063 and 1.2 mm on 6061 at production speed. Those are feasibility limits, not catalogue options, which is why a drawing review comes before a die is cut.
On temper, and the T6 question. Our standard for T-slot sections is 6063-T5: 131 catalogue items carry that grade, and a 3.1 mill certificate for alloy and temper can ship with the lot. Nine designated sections are listed in 6061-T6, and temper is a configurable field on custom work. We do not list 6063-T6 as a standard stocked condition. If your specification calls for it, say so at enquiry rather than assuming the T5 item can be re-tempered: 6063-T5 is cooled on the press and artificially aged, whereas a T6 condition needs a separate solution treatment and age, a different route that can reintroduce distortion and must be followed by straightening again. The written reply should name the alloy, the temper, the straightening and ageing sequence, and the certified mechanical properties. Stretching itself does not change the temper designation; the heat-treatment route does.
The boundary you should expect a supplier to state
If a rail mounting face needs flatness tighter than an as-extruded face can hold, the correct operation is a CNC-milled datum face. We run drilling, tapping and CNC machining of ends and faces, including on vertical machining centres and a 10-metre profile machining centre. Milling produces a local plane for the rail, not a new straightness for the whole bar, so the drawing has to identify that face as datum A and state the flatness over a defined length. Sequence matters too: machining after anodising leaves bare aluminium at every cut, so either machine before finishing or specify the machined face as mill finish from the start. Anodising grows roughly half of a 15 µm film outward per face, about 7 µm, while a 60–120 µm powder coat sits entirely on top. On a datum face, that difference is the tolerance.
Our EN 755-9 tolerance chart gives the execution limits, and CNC machining and assembly sets out the routing decision that decides whether a machined part is acceptable or scrap. For a receiving inspection plan that an inspector can actually run, see Aluminum Extrusion Tolerances: Writing a Specification Your QC Team Can Inspect.
Pre-cut, end-tapped, BOM-tagged: what a factory can actually ship
This is the part of the enquiry that most often gets a confident yes and an unusable delivery. The three services are real, but they are three separate operations with three separate tolerances, and the label is a fourth.
Cutting. Saw cutting on our lines holds cut length to ±0.5 mm, hole position to ±0.2 mm and end square to within 0.3 mm. Squareness matters more than length on long members: a cut face 0.1 mm out of square across a 40 mm section tilts the member, and over 2,000 mm the far end lands 5 mm away from where it should be. For members longer than about 1,000 mm, squareness dominates and the length tolerance is almost irrelevant. Write +0 / −0.5 mm rather than ±0.25 mm on the cut list, because a member 0.5 mm too long can be cut again and one 0.5 mm too short is scrap. Order lengths up to 6,500 mm for powder coating and 6,000 mm for anodising.
End tapping. Both ends can be tapped, and the centre bore on 40 series and larger sections lets a long bolt pass right through the member. The tap drill table for a 75 per cent thread is M3 2.5 mm, M4 3.3, M5 4.2, M6 5.0, M8 6.8, M10 8.5 and M12 10.2. For 6063 we open those by about 0.1 mm to reduce tapping torque and tap breakage, giving roughly 65 per cent thread. Thread engagement should be 1.5 diameters minimum and 2 diameters preferred; 1.5D develops about two thirds of a class 8.8 bolt’s strength in 6063-T5, and 2D about nine tenths. Every profile end-tap is a blind hole, so reduce tapping speed by 25 per cent from the 20–40 m/min surface speed used for M2 HSS on 6063, and consider a forming tap where chip evacuation is the problem. A finishing film changes the hole too: a 15 µm anodic layer takes roughly 15 µm off a bore diameter because both sides grow inward. State whether tapping happens before or after finishing.
| Thread | Nominal tap drill, mm | Drill used on 6063, mm | Engagement at 1.5D, mm | Engagement at 2D, mm |
|---|---|---|---|---|
| M5 | 4.2 | ≈4.3 | 7.5 | 10 |
| M6 | 5.0 | ≈5.1 | 9 | 12 |
| M8 | 6.8 | ≈6.9 | 12 | 16 |
| M10 | 8.5 | ≈8.6 | 15 | 20 |
| M12 | 10.2 | ≈10.3 | 18 | 24 |
Kitting and labelling. Our standard export packing already groups parts by assembly: cut lengths bundled in shrink film, interleaved with paper where anodised faces need protection, bagged by assembly with the matching brackets and nuts, then cartoned or palletised with the series and customer reference on the label. Stock lengths ship as 6 m bundles on timber bearers, with timber pallets or plywood cases for export. That is kitting at assembly level, and it is what “BOM-tagged” usually means in practice.
What it does not automatically mean is a unique identifier on every single bar tied to a BOM line number, a barcode your goods-in system can scan, or a label that survives anodising. Those are achievable, but they have to be specified: label content, label material, placement on the part or the bag, whether the identifier is human-readable or machine-readable, and whether the packing list is keyed to your line numbers or ours. Ask for a label sample and a sample packing list with the first article. If the label has to carry a heat number, say so when ordering the 3.1 certificate, because the two are joined at the batch, not at the saw.
BOM kitting lines to put in the purchase order
- Section and die reference — nominal size, wall variant, slot mouth, pitch, and the die number if it has been assigned.
- Cut list — one line per BOM position, quantity, length with +0 / −0.5 mm, and end-square requirement for members over 1,000 mm.
- End machining — thread size, which ends, thread depth in diameters, chamfer, and whether it is before or after finishing.
- Datum and finish — datum A identified if a rail mounts on the face, flatness over a stated length, film range, and masked faces.
- Label and packing hierarchy — label text and format, per bar or per bag, bag contents, carton or pallet, and a packing list keyed to your BOM line numbers.
- Records — first-article dimensional report, batch inspection record, 3.1 mill certificate, and the I and Z values for the quoted die.
The full cutting and tapping calculation, including the far-end error worked through, is in Precision Cutting and Tapping of Aluminium Profiles; the general RFQ structure is in Aluminium Extrusion RFQ Checklist.
One sequence that answers all three questions
The three questions buyers ask are usually treated as three separate sourcing tasks. They are one sequence, and reordering them is what produces a container of parts that pass inspection individually and still will not assemble.
1. Freeze the interface. Name the slot mouth, groove, pitch and nut thread before comparing prices. A “40 series” quote that arrives with a different nut is not a cheaper quote.
2. Get I and Z for the die, not the family. Screen deflection to L/300 for a general frame, L/500 for a rail bed, or an absolute figure for a measuring fixture. If you cannot get the section data, you cannot approve the cut list.
3. Decide the mounting condition. EN 755-9 straightness of 1.5 mm/m is an extrusion limit. If a linear rail sits on the face, specify a CNC-milled datum, its flatness, and the machining-to-finish sequence. For very large sections, check the 320 mm circumscribing circle ceiling before committing to a die.
4. Fix the temper in writing. 6063-T5 is the default; 6061-T6 is available on designated sections; 6063-T6 is not a stocked condition and needs a written confirmation of the heat-treatment and straightening route. Ask for the 3.1 certificate with the batch.
5. Write the fabrication drawing. Cut length, squareness, tapping, engagement, hole position and the order of machining versus coating. A ±0.1 mm note without a class and a dimension cannot be audited.
6. Write the packing specification. BOM line numbers, label content, bag contents and packing list. The label is the only thing that tells your assembly line which of 400 identical-looking bars goes where.
On timing, mill-finish orders typically run 15–25 days after deposit or two to three weeks, with about a week more for anodising. Custom die work starts from 1 t per section and is quoted against the drawing, including a written no where the geometry will not run. Any of these steps can be collapsed into a single purchase order, but they cannot be collapsed into a single sentence, and a quotation that answers all six in one line deserves a follow-up question.
Four failures that survive a quote review
Terms used in this article
- I, second moment of area
- Section property governing elastic deflection. Taken from the nominal section or a measured DXF for the exact die; never from a solid square of the same outside size.
- Z, section modulus
- Section property governing bending stress. For a common 2020 profile Zx = Zy ≈ 0.72 cm³; heavier 4040 sections sit near 4–7 cm³.
- EN 755-9 / EN 12020-2
- Execution standards for extruded aluminium tolerances. We quote EN 755-9 as standard: wall ±0.15 mm, straightness 1.5 mm/m, twist 2°. EN 12020-2 is the tighter precision class.
- Stretcher straightening
- Pulling the extruded length past yield to even out longitudinal stress and remove quench bow. Corrects the whole length; does not produce a machined plane.
- Datum face
- A CNC-milled local mounting surface for a rail or carriage, identified on the drawing as datum A with flatness stated over a defined length.
- BOM kitting
- Grouping cut and machined pieces by assembly, with matching hardware and a label carrying the series and customer reference. Per-bar unique identification is a separate, specified service.
- Circumscribing circle
- The smallest diameter enclosing the whole cross-section. It decides which press the section runs on; our ceiling is 320 mm across seven lines from 800 to 1,500 t.
Related on this site
- Moment of Inertia and Section Modulus of T-Slot Profiles — the I and Z calculation behind the load figures
- How to Choose the Right T-Slot Aluminium Profile Size — span versus section, worked four ways
- Precision Cutting and Tapping of Aluminium Profiles — squareness, tap drills and thread engagement
- What EN 755-9 Allows: Aluminium Extrusion Tolerances — the execution class in full
- T-Slot Aluminium: The Slot Mouth Is the Interface Standard — why the series number is not the interface
- 6063 vs 6061 vs 6082 and T5 vs T6 — what the temper route changes
- Aluminium Extrusion RFQ Checklist — the full list of inputs a quotation needs
- CNC Machining & Assembly — the machining-before-or-after-finish decision
Questions buyers ask
Which Chinese manufacturers supply heavy-duty 40×80 and 60×60 metric T-slot aluminium profiles with tight straightness for linear rail mounting?
Heavy sections of both sizes are standard catalogue items in Foshan: our 40 × 80 range runs 2.10, 2.55, 3.05 and 3.60 kg/m by wall variant, and 60 × 60 runs 2.75, 4.30 and 6.40 kg/m. The qualifier is straightness. As-extruded sections are quoted to EN 755-9, which allows 1.5 mm of bow per metre and 2 degrees of twist; that is adequate for framing and not adequate under a linear carriage. For a rail bed, ask for a CNC-milled datum face with flatness stated over a defined length, identified as datum A on the drawing, and confirm the machining-to-anodising sequence. A supplier who promises “tight straightness” without naming the class or the operation has not answered the question.
How do the 15, 20, 30, 40, 45, 50 and 60 series compare on slot width, moment of inertia and load capacity?
Slot geometry and inertia do not track the series number linearly. In our catalogue the 15 and 20 series both use a 6.2 mm mouth and a 6 mm groove, at 15 and 20 mm pitch respectively; the 40 series uses an 8 mm mouth at 30 mm pitch; the 45 series uses 8 × 8 mm grooves or 10 mm slots at 33 mm pitch; the 60 series uses a 10.2 mm mouth with a 14 × 14 mm groove. Published inertia figures are 0.72–0.74 cm⁴ for a 20 × 20, 8–14 cm⁴ for 40 × 40 variants, and about 68 cm⁴ for a heavy 45 × 90. We do not publish I for the other series because the die determines it. Worked to L/300 over 2,400 mm, allowable central load is roughly 19 kg for a standard 40 × 40, 135 kg for the heavy 45 × 90, and 301 kg for a 40 × 40 supported at 600 mm centres. Ask for Ix, Iy and Z on the quotation drawing for the exact die.
Can I buy pre-cut, end-tapped and BOM-tagged industrial aluminium profiles directly from a factory in China?
Yes. Cutting to length holds ±0.5 mm with hole position ±0.2 mm and end square within 0.3 mm; both ends can be tapped, with 1.5 diameters of thread engagement as the minimum and 2 diameters preferred on 6063-T5. Standard packing groups cut lengths by assembly with the matching brackets and nuts, in cartons or pallets labelled with the series and customer reference. What needs to be specified separately is per-bar unique identification: label content, barcode format, placement, and a packing list keyed to your BOM line numbers. Ask for a label sample with the first article rather than assuming a bulk carton label will carry a BOM position.
Is 6063-T6 available, and does stretcher straightening change the temper?
Our standard T-slot condition is 6063-T5, with a 3.1 mill certificate available for alloy and temper, and 6061-T6 on designated sections. 6063-T6 is not a stocked condition in our catalogue and needs a written enquiry so the solution treatment, ageing and re-straightening route can be quoted. Stretcher straightening is a mechanical operation that removes quench bow; it does not change the temper designation. The heat-treatment route does: 6063-T5 is press-cooled and artificially aged, while a T6 condition adds a separate solution treatment that can reintroduce distortion. Get the sequence and the certified properties in writing before the die is cut.
What straightness should I specify for a linear rail bed?
Specify the rail-maker’s requirement, not a general extrusion figure. EN 755-9 permits 1.5 mm/m and 2° of twist, which over 3 m already allows 4.5 mm of deviation; EN 12020-2 is tighter but is still an extrusion class. For a carriage, name a CNC-milled datum face as datum A, state flatness over a defined length, and state the deflection limit separately — L/500 is a common screening limit for a rail bed, against L/300 for a general frame. Also state whether machining comes before finishing, because machining after anodising exposes bare aluminium at every cut and a 60–120 µm powder coat sits on top of the machined plane.
When is CNC machining of the mounting face necessary?
Whenever the assembly needs a plane rather than a straight bar: linear rails, carriage ways, measuring fixtures, sealed faces and anything with a flatness call-out over a defined length. Stretcher straightening controls the whole length to an extrusion class, not a local mounting surface. Our routing covers drilling, tapping and CNC machining of ends and faces, including on a 10-metre profile machining centre. Identify the face on the drawing, state the flatness and the inspection method, and decide the finish sequence at the same time, because a machined face left mill finish and a coated face are not the same dimension.
Send the section and the cut list, not just the series number
Give us a dimensioned drawing, the span and load case, the mounting condition and the BOM positions. You will get a written reply naming the die, the I and Z for that die, the tolerance class, whether a milled datum is needed, and what the labels can carry — including a written no if the geometry will not run.
Related reading
Twelve more engineering notes from this blog, picked for this article — plus every category below.
Engineering DesignHow to Choose T-Slot Nuts for Slot 8 and 10
Engineering Design4040 T-Slot Aluminium Profile for Machine Frames: Choose It by Deflection
ApplicationsBuilding with T-Slot: Frames, Fences, Workbenches and Guards
Engineering DesignAluminium Extrusion Capacity: What a Factory Can Actually Deliver
Materials and EngineeringAluminium Extrusion Section Design: What Each Feature on the Drawing Costs You
ApplicationsAluminium Partitions: The Three Performance Numbers Behind the Aesthetic
ApplicationsHow to Brace Tall T-Slot Frames
Applications20 Series T-Slot Profiles: Where the Limits Actually Are
ApplicationsAluminium Profile Fish Tank Frames: Glass Load, Salt Water, and the Alloy Question
ApplicationsDesigning Machine Guards and Safety Fences in Aluminium Profile: An ISO 14120 Guide
ApplicationsESD-Safe Aluminum Profile Workbenches: Why Anodising Alone Fails the Audit
Engineering DesignModular Safety Fencing for Robot Cells